[email protected]

ASTM A358 Stainless Steel TP304, 304L, 304H CL.1 EFW Pipes

Tensile Strength:Yield Strength (0.2%Offset) Elongation:SS 304/304L/304H:8.0 g/cm3:1400 °C (2550 °F) Psi 75000, MPa 515:Psi 30000, MPa 205:40 % Mechanical properties of Austenitic Stainless Steel 304L Jan 01, 2016 · As it can be seen from the table, the R value for % elongation of ASS 304L is 0.9014 and for n is 0.8625, but the value of average absolute error is 6.6% and 5.8%, respectively. This clearly shows that even though the R value is higher for % elongation, the error value is also higher as compared to n.

SS304 / SS304L

The low carbon content restricts carbide precipitation during welding as well as minimizes its susceptibility to intergranular corrosion. Stainless steel 304L (SS304L) is an extra low-carbon variation of SS304 with a 0.03% maximum carbon content that eliminates carbide precipitation due to welding. Both SS304 and SS304L have excellent resistance to a wide range of atmospheric, chemical and petrochemical, and STAINLESS STEEL Grade 304, 304L, 304HTensile Strength [MPa] 0.2% Proof Stress [MPa] Elongation [% ] Impact Energy [J] 20 616 255 70 217 0 885 242 64 204-10 976 240 55 194-50 1101 236 50 194-100 1281 222 42 168-140 1368 246 41 160-196 1609 231 38 168 STAINLESS STEEL Grade 304, 304L, 304H Representative Creep Rupture Properties:Properties at Sub-Zero Temperatures FATIGUE PROPERTIES Stainless 316, 316L, 317, 317LIn addition to excellent corrosion resistance and strength properties, the Types 316, 316L, 317, and 317L Cr-Ni-Mo alloys also provide the excellent fabricability and formability which are typical of the austenitic stainless steels. Specifications. Chemical Composition, % 18. Resistance to Corrosion:304, and 304L, will not attack these molybdenum

Stainless Steel 304L - 1.4307 Data Sheet

Stainless steel 304 and 304L are also known as stainless steel 1.4301 and 1.307 respectively. Type 304 is the most versatile and widely used stainless steel. It is still sometimes referred to by its old name 18/8 which is derived from the nominal composition of type 304 being 18% chromium and 8% nickel. Type 304 stainless steel is an austenitic grade that can be severely deep drawn. Stainless Steel Plate 304 304L ASTM A240 - Penn StainlessIt is important to understand the mechanical properties of 304 and 304L stainless steel plate, ASTM A240. 304 stainless steel plate has a minimum tensile strength of 75 ksi and a minimum yield strength at 0.2% of 30 ksi. 304 stainless steel plate has an elongation of 40%. This type of stainless steel plate has a maximum Brinell hardness of 201 Stainless Steel Type 304-304L Tempered & Specialty Metals304L:Yield Strength, min. (ksi) 30:25:Tensile Strength, min. (ksi) 75:70:Elongation, min. (%) 40:40:Hardness, max. (Rb) 92:92

AISI Type 304L Stainless Steel

Tensile Strength, Ultimate :564 MPa:81800 psi:0% Cold-worked:Tensile Strength, Yield :210 MPa:30500 psi:0% Cold-worked:Elongation at Break :58 %:58 %:In 50mm (2 in.) Modulus of Elasticity :193 - 200 GPa:28000 - 29000 ksi:Charpy Impact :216 J:159 ft-lb :Electrical Properties Metric English Comments; Magnetic Permeability :1.008